空气等离子喷涂板式SOFC连接体保护涂层的性能
引用本文:付长璟 孙克宁 张乃庆 周德瑞. 空气等离子喷涂板式SOFC连接体保护涂层的性能[J]. 稀有金属材料与工程, 2006, 35(7): 1117-1120
作者姓名:付长璟 孙克宁 张乃庆 周德瑞
作者单位:哈尔滨工业大学应用化学系,黑龙江,哈尔滨,150001
基金项目:国家新技术研究发展基金(863计划)
摘    要:在中温平板型固体氧化物燃料电池(ITSOFC)设计中,可以采用金属作为连接材料.Fe-16Cr合金是较为理想的金属连接材料,它存在的主要问题是连接体阴极侧表面的高温氧化和腐蚀,会导致电池性能的迅速降低.本研究采用空气等离子喷涂的方法喷涂了La0.8Sr0.2MnO3-σ(LSM)钙钛矿型保护涂层在金属连接板的表面,并讨论了主要过程参数及其作用效果.研究发现,喷涂后热处理是降低涂层孔隙率的有效方法,经喷涂-热处理后,涂层的孔隙率可降至1%以下.等离子喷涂LSM保护涂层后,Fe-16Cr合金的耐高温氧化性能明显提高,氧化速率降低了76%.

关 键 词:固体氧化物燃料电池  连接体  空气等离子喷涂  La0.8Sr0.2MnO3-σ  热障涂层  La0.8Sr0.2MnO3-σ
文章编号:1002-185X(2006)07-1117-04
收稿时间:2005-04-27
修稿时间:2005-04-27

Effects of Protective Coating Prepared by Atmospheric Plasma Spraying on Planar SOFC Interconnect
Fu Changjing,Sun Kening,Zhang Naiqing,Zhou Derui. Effects of Protective Coating Prepared by Atmospheric Plasma Spraying on Planar SOFC Interconnect[J]. Rare Metal Materials and Engineering, 2006, 35(7): 1117-1120
Authors:Fu Changjing  Sun Kening  Zhang Naiqing  Zhou Derui
Affiliation:Department of Applied Chemistry, Harbin Institute of Technology, Harbin 150001, China
Abstract:In the planar design of intermediate temperature solid oxide fuel cell (ITSOFC), a metallic interconnect is used to separate the single cells. Fe-16Cr alloy is a promising metallic interconnect material and a disadvantage of it is the high-temperature oxidation and corrosion at the surface of the cathode side leading to rapid cell degradation. In this paper, a dense La0.8Sr0.2MnO3-σ (LSM) perovskite coatings were deposited on the surfaces of the metallic interconnects prepared by atmospheric plasma spraying (APS). The main process factors and their effect on protective coatings were discussed. The appropriate process parameters were determined in the experiment. It was found that heat treatment after APS is an effective method for reducing the porosity in the coating. After heat-treatment, the LSM coatings with porosity with less than 1% were obtained. By spraying LSM protective coatings, the oxidation rate of Fe-16Cr alloy in air at 1073 K was lowered by 76%.
Keywords:SOFC  interconnect  APS  coating