Abstract: | The strength of dense high-slag cement-sand mixes autoclaved at 180 lbf/in2, and of certain aerated mixes autoclaved at pressures ranging from 120 to 210 lbf/in2, has been determined. It was found that maximum strengths were developed in an autoclaving period of 5 h at 180 lbf/in2, and that longer periods, as well as higher autoclaving pressures, yielded lower strengths. The maximum strength values obtained for compacted 1: 3 (w/w) mixes were 425 kg/cm2 in the absence of fine quartz, and 510 kg/cm2 in the presence of suitable addition of fine quartz. The corresponding values for Portland cement mixes were, respectively, 330 and 460 kg/cm2 for a heating period of 5 h, and 360 and 505 kg/cm2 for a period of 6 h. |