30 t EAF-40 t LF冶炼35MnVS 易切削钢的工艺实践
引用本文:李艾,刘光辉,朱志欣,王秀兰. 30 t EAF-40 t LF冶炼35MnVS 易切削钢的工艺实践[J]. 特殊钢, 2005, 26(4): 54-55
作者姓名:李艾  刘光辉  朱志欣  王秀兰
作者单位:东北特钢集团北满特殊钢有限责任公司,齐齐哈尔161041
摘    要:采用30tEBTEAF40tLF(喂线)3.15t铸锭工艺生产35MnVS易切削钢(%):0.33~0.40C,0.30~0.60Si,1.00~1.40Mn,0.06~0.12V,≤0.035P,0.035~0.075S。30炉35MnVS钢的生产结果表明,LF精炼时,喂硫磺粉线前钢中的硫含量为0.007%~0.032%,喂硫磺粉线后钢中硫含量为0.040%~0.071%,喂丝硫的回收率为50%~80%。喂硫线后,再喂入0.3kg/t的铝线,细化钢的晶粒。35MnVS易切削钢成品材的晶粒度为6~7级,钢的机械性能和高、低倍组织均满足标准要求。

关 键 词:35MnVS易切削钢     LF精炼  喂线  
收稿时间:2005-02-16

Practice of Free Cutting Steel 35MnVS Steelmaking by 30 t EAF-40 t LF
Li Ai,Liu Guanghui,Zhu Zhixin,Wang Xiulan. Practice of Free Cutting Steel 35MnVS Steelmaking by 30 t EAF-40 t LF[J]. Special Steel, 2005, 26(4): 54-55
Authors:Li Ai  Liu Guanghui  Zhu Zhixin  Wang Xiulan
Affiliation:Beiman Special Steel Co Ltd,Dongbei Special Steel Group, Qiqjhaer 161041
Abstract:The free cutting steel 35MnVS- 0.33~0.40C,0.30~0.60Si,1.00~1.40Mn,0.06~0. 12V, ≤0.035P,0.035~0.075S was produced by 30 t EBT EAF-40t LF (wire feeding)- 3.15 t ingot casting process. The production results of 30 heats steel 35MnVS showed that the sulphur content in steel after sulphur powder wire feeding was 0.040%-0.071%, while before feeding that was 0.007%~0.032%;and the sulphur yield of wire feeding was 50%~ 80%.The 0.3 kg/t aluminum wire was feeding after sulphur wire feeding to fine the grain size of steel. The grain size rating of 35MnVS products was 6~7, and the mechanical properties, micro- and macro structure met the standard requirements.
Keywords:Free Cutting Steel 35MnVS   LF Refining   Wire Feeding
本文献已被 CNKI 维普 万方数据 等数据库收录!
点击此处可从《特殊钢》浏览原始摘要信息