氢一次还原钨粉烧结多孔构件的工艺研究
引用本文:孙百顺.氢一次还原钨粉烧结多孔构件的工艺研究[J].粉末冶金技术,1988,6(1):37-42.
作者姓名:孙百顺
作者单位:航天工业部第四十三研究所
摘    要:研究了氢一次还原、平均粒度为6.5—7.5μm的钨粉的烧结特性。得出多孔钨构件的相对密度随烧结温度和时间、粉末粒度、压制件密度而变化的规律。提出了生产相对密度为78—81%、开孔率>95%的多孔钨的生产工艺参数,即:压制件相对密度为60—65%,烧结温度为2100—2250℃、时间为4—8小时。


A STUDY OF POROUS COMPONENTS MADE BY TUNGSTEN POWDER PRODUCED BY SINGLE REDUCTION PROCESS OF HYDROGEN
Affiliation:Research Institute No. 43 of the ministry of Airospece Industry
Abstract:Sintering characteristics of tungsten powder with mean particle size of 6.5 to 7.5μm singly reduced by hydrogen have been investigated.It is concluded that the relative density of porous tungsten components varies with the sintering temperature and time, particle size and green density. The parameters for producing porous tungsten products with relative density in a range of 78-81% and open porosity over 95% are outlined as follows; relative density of compacts-60-65%, sintering temperature 2100-2250℃ and sintering time-4~8 hours.
Keywords:
本文献已被 CNKI 等数据库收录!
点击此处可从《粉末冶金技术》浏览原始摘要信息
点击此处可从《粉末冶金技术》下载全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号