摘    要:以螺环磷酰二氯(SPDPC)与哌嗪为原料,在未加溶剂和催化剂的条件下,用高速万能粉碎机粉碎混合原料的同时,借助转刀高速旋转的剪切力所产生的热能加热体系发生反应,合成了螺环磷酰哌嗪酯。分析了原料摩尔比以及混合时间对产品得率的影响,得出了较优的反应条件:n(螺环磷酰二氯)∶n(哌嗪)=1∶2,混合时间350s,在该条件下得到暗白色粉末状固体,产率达95%以上。产品用红外光谱和核磁共振波谱进行了表征。

关 键 词:螺环磷酰二氯  哌嗪  固相反应  阻燃剂  橡塑助剂
收稿时间:2012/1/11 0:00:00
修稿时间:2012/2/13 0:00:00

Spirocyclic Piperazine Phosphate Synthesized in Solid Phase
suncaiying,Zhan Zhaoshun and Liu Xiangyang.Spirocyclic Piperazine Phosphate Synthesized in Solid Phase[J].Fine Chemicals,2012,29(5):495-498.
Authors:suncaiying  Zhan Zhaoshun and Liu Xiangyang
Affiliation:Department of chemistry, Northeast Forestry University;Heilongjiang key laboratory of molecular design and preparation of flame retarded materials,Department of chemistry, Northeast Forestry University;Heilongjiang key laboratory of molecular design and preparation of flame retarded materials
Abstract:With spirocyclic phosphate,3,9-dichloro-2,4,8,10-tetraoxa-3,9-diphosphasprio undecane-3,9-dioxide(SPDPC) and piperazine as raw materials,which were mixed and ground in a high-speed multi-functional grinder,and with no solvent and catalyst in presence,spirocyclic piperazine phosphate was synthesized under the heat energy produced by the high-speed shear strength of the grinder′s rotating knife.The effect of the mole ratio of raw materials and the mixing time on the yield of the final product was studied and the optimum reaction conditions were identified.The yield of the final product in the shape of fuzzy white powder reached more than 95% when SPDPC and piperazine were mixed for 350 s in molar ratio 1∶2.The structure of the product was characterized by means of IR and NMR.
Keywords:SPDPC  piperazine  solid-phase reaction  flame retardant  rubber and plastics auxiliaries
本文献已被 CNKI 万方数据 等数据库收录!
点击此处可从《精细化工》浏览原始摘要信息
点击此处可从《精细化工》下载全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号