Hermetic Packaging Using Eutectic SnPb Solder and Cr/Ni/Cu Metallurgy Layer
Authors:Huang   A. T. Chou   C.-K. Chen   C.
Affiliation:Dept. of Mater. Sci. & Eng., Nat. Chiao Tung Univ., Hsinchu;
Abstract:We have developed an easy, low-cost, and low-temperature optoelectronic hermetic packaging technology utilizing the eutectic SnPb solder and the Cr/Ni/Cu bonding pad. Bonding characteristics of the design were investigated in three different setups: silicon-silicon, silicon-glass, and glass-glass samples. Hermeticity was achieved at 200 degC without flux for all samples during the final bonding process. The bonding pads did not dewet during or after the reflow process. By utilizing the eutectic SnPb solder, the self-alignment process can be achieved. Because the bonding process was conducted through visual alignment, original misalignment was estimated to be more than 100 mum. The surface tension of melting solder during the reflow process allowed the samples to self-align and obtain a misalignment of less than 20 mum after solidification, which was 4% of the entire solder width. The bonding strength of the three setups ranged from 3 to 10 MPa. Among the three setups, glass-glass samples appear to have the strongest bonding strength. This low-temperature and cost-effective soldering process has demonstrated its feasibility and potential utilization in optoelectronic packaging
Keywords:
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号