后盖外板上部冲压工艺改进
引用本文:刘罡,程迎潮,江谷明,武朋飞. 后盖外板上部冲压工艺改进[J]. 锻压技术, 2009, 34(6). DOI: 10.3969/j.issn.1000-3940.2009.06.015
作者姓名:刘罡  程迎潮  江谷明  武朋飞
作者单位:上海大众汽车有限公司模具中心,上海,201805
摘    要:后盖外板上部型面复杂,局部特征多,冲压工艺采用6道工序完成,试模过程中第5道工序的工件严重起皱,影响表而质茸及焊接工艺性.经过分析,发现该缺陷主要是由不合理的整形工艺造成的,为此,对整形斜楔进行了改进,增加了一块小压料板,在整形面上添加吸料槽,并重新设计了整形块的结构.经过改进,基本消除了起皱,零件质量得到了显著提高.

关 键 词:后盖外板  冲压工艺  整形

Stamping process improvement of rear cover outer top
LIU Gang,CHENG Ying-chao,JIANG Gu-ming,WU Peng-fei. Stamping process improvement of rear cover outer top[J]. Forging & Stamping Technology, 2009, 34(6). DOI: 10.3969/j.issn.1000-3940.2009.06.015
Authors:LIU Gang  CHENG Ying-chao  JIANG Gu-ming  WU Peng-fei
Abstract:The shape of rear cover outer top is very complicated, and there are many local features. The stamping process is of six operations. During try-out, serious wrinkle had occurred in the fifth operation, which would damage surface quality and result in bad weldable. It was found that unreasonable restrike process is the main causation. Therefor, the restrike CAM was improved. First, a small pad was added. Second, material absorbing groove was add-ed on the surface. Then, the structure of restrike block was re-designed. By means of these methods, wrinkle was uhi-mately eliminated and part's quality was evidently improved.
Keywords:rear cover outer  stamping process  restrike