摘    要:云南某硫化铅锌矿中Pb的品位为6.82%、Zn的品位为21.03%,主要脉石矿物是方解石、白云石等,且矿石中含黄铁矿较多,对铅锌选矿造成一定的影响.对该矿采用优先浮选的工艺流程,通过条件试验确定各浮选作业的最佳技术参数.最终,通过铅硫混选选铅,铅硫混选产品进行铅硫分选,铅硫分选尾矿进行锌硫分选,中矿依次返回上一作业;选...

关 键 词:铅锌矿  选矿  铅精矿  锌精矿
收稿时间:2020-10-30
修稿时间:2020-12-09

Experimental Study on Beneficiation of a Lead Zinc Sulfide ore in Yunnan
SUBHONQULOV SUBHONQUL,liuquanjun and dongjingshen. Experimental Study on Beneficiation of a Lead Zinc Sulfide ore in Yunnan[J]. Nonferrous Metals Engineering, 2021, 0(4): 78-87
Authors:SUBHONQULOV SUBHONQUL  liuquanjun  dongjingshen
Affiliation:Kunming University of Science and Technology, Faculty of Land Resources Engineering,Kunming University of Science and Technology, Faculty of Land Resources Engineering,Kunming University of Science and Technology, Faculty of Land Resources Engineering
Abstract:A lead-zinc sulfide ore in Yunnan assays grade of 6.82% Pb and 21.03% Zn. The main gangue minerals are calcite, dolomite and so on, and the ore contains a lot of pyrite, which has a certain impact on Lead-Zinc beneficiation. In this paper, the flotation process is adopted and the optimal technical parameters of each flotation operation are determined through condition test. Finally, lead is selected through lead sulfur mixed separation, lead and sulfur mixed separation products were selected for lead and sulfur separation. Zinc and sulfur are separated from tailings of lead and sulfur separation. Middlings are returned to the previous operation in turn, and the middlings of "one roughing and three scavenging" of zinc are returned to the closed-circuit test process of the previous operation in turn. Through the addition of redesigned reagents and the adoption optimized process flow. The qualified lead concentrate with lead content of 66.1% and recovery rate of 88.95% is obtained. The sulfur content in the sulfur concentrate is 50.11% and the iron content is 42.91%, which effectively inhibits pyrite. The qualified zinc concentrate with zinc content of 61.6% and recovery rate of 95.16% was obtained. At the same time, the silver content in the lead concentrate was 410.9 g/t. The silver in the ore has been effectively enriched. The comprehensive utilization of metal is realized effectively.
Keywords:Lead zinc ore   mineral processing   lead concentrate   zinc concentrate
本文献已被 CNKI 维普 等数据库收录!
点击此处可从《有色金属工程》浏览原始摘要信息
点击此处可从《有色金属工程》下载免费的PDF全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号