Degradation phenomena in PEM fuel cell with dead-ended anode
Authors:Toyoaki Matsuura  Jixin ChenJason B Siegel  Anna G Stefanopoulou
Affiliation:Department of Mechanical Engineering, University of Michigan, 2350 Hayward St., Ann Arbor, MI 48109, USA
Abstract:To improve the performance and durability of a dead-ended anode (DEA) fuel cell, it is important to understand and characterize the degradation associated with the DEA operation. To this end, the multiple degradation phenomena in DEA operation were investigated via systematic experiments. Three lifetime degradation tests were conducted with different cell temperatures and cathode relative humidities, during which the temporal evolutions of cell voltage and high frequency resistance (HFR) were recorded. When the cathode supply was fully humidified and the cell temperature was mild, the cathode carbon corrosion was the predominant degradation observed from scanning electronic microscopy (SEM) of postmortem samples. The catalyst layer and membrane thickness were measured at multiple locations across the cell active area in order to map the degradation patterns. These observations confirm a strong correlation between the cathode carbon corrosion and the anode fuel starvation occurring near the cell outlet. When the cathode supply RH reduced to 50%, membrane pin-hole failures terminated the degradation test. Postmortem analysis showed membrane cracks and delamination in the inlet region where membrane water content was the lowest.
Keywords:Fuel cell degradation  Dead-ended anode  Carbon corrosion  Membrane pin-hole
本文献已被 ScienceDirect 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号