使用PE隔板的摩托车电池的早期失效方式
引用本文:郭志刚.使用PE隔板的摩托车电池的早期失效方式[J].蓄电池,2006,43(3):139-142.
作者姓名:郭志刚
作者单位:保定风帆摩托车蓄电池有限公司,河北,保定,071057
摘    要:通过与使用PE隔板汽车电池失效方式的对比,重点分析了摩托车电池的早期失效方式,深入探讨了由于PE隔板问题造成的摩托车电池的失效原因,提出控制极板质量、在电解液中添加硫酸钠或硫酸镁以及提高PE隔板的渗透性和抗刺穿强度的解决方案。

关 键 词:PE隔板  摩托车电池  失效方式
文章编号:1006-0847(2006)03-0139-04
修稿时间:2005年4月12日

Discussion on the premature failure modes of motorcycle batteries with PE separators
GUO Zhi-gang.Discussion on the premature failure modes of motorcycle batteries with PE separators[J].Chinese Labat Man,2006,43(3):139-142.
Authors:GUO Zhi-gang
Abstract:As compared with the case of car batteries,the failure modes of motorcycle batteries with PE separators were analysed emphatically,and the failure modes resulted from PE separators were discussed in detail.Additionally,the following measures were taken to solve the problems:controlling the plate quality;adding Na_2SO_4 or MgSO_4 into the electrolyte and improving the penetrability and penetration resistance of PE separators.
Keywords:PE separator  motorcycle battery  failure mode