首页 | 本学科首页   官方微博 | 高级检索  
     

云南某钨锡矿选矿试验研究
引用本文:李伟. 云南某钨锡矿选矿试验研究[J]. 中国矿业, 2014, 23(6)
作者姓名:李伟
作者单位:云南锡业集团有限责任公司研究设计院
摘    要:云南某钨锡矿含钨0.323%,锡0.140%,二氧化硅63.13%,三氧化二铝17.44%,氧化钙2.92%,氧化镁2.44%,在矿石工艺矿物学及试验研究的基础上,采用一段磨至-0.5mm,针对不同的床型,开展水力分级,进行摇床粗选,混合精矿脱硫、除铁、常温浮选分离钨锡的选矿工艺,获得了钨精矿产率0.31%,钨品位71.06%,钨回收率67.69%,含锡0.56%;锡精矿产率0.12%,锡品位58.18%,锡回收率50.94%,含钨3.80%,锡富中矿产率0.21%,锡品位4.22%,锡回收率6.87%,含钨2.69%,综合锡回收率57.81%的技术指标。

关 键 词:白钨矿  锡石 摇床粗选  钨锡分离
收稿时间:2013-10-28
修稿时间:2014-02-27

Separation Experiment of a Wolfram and Tin Ore in Yunnan
liwei. Separation Experiment of a Wolfram and Tin Ore in Yunnan[J]. CHINA MINING MAGAZINE, 2014, 23(6)
Authors:liwei
Abstract:A Wolfram and Tin Ore of Yunnan containing Tungsten 0.323%,Tin 0.140%,Silicon dioxide 63.13%,Aluminum oxide 17.44%, Calcium oxide 2.92%, Magnesium oxide 2.44%. This Paper based on the study on ore mineralogy and experiment, used the mineral processing technology of a grinding to -0.5mm, according to the different types of bed, development of hydraulic classification, rough selection of shaking table, mixed concentrate desulphurization, removal of iron, W-Sn separation flotation at normal temperature. The experiment technical indexes were: the yield of tungsten concentrate 0.31%, Tungsten grade of 71.06%, recovery rate of Tungsten 67.69%, Tin containing 0.56%; the yield of Tin concentrate 0.12%, Tin grade of 58.18%, recovery rate of Tin 50.94%, tungsten containing 3.80%; the yield of Tin middling 0.21%,tin grade of 4.22%, recovery rate of tin 6.87%, tungsten containing 2.69%, comprehensive recovery rate of Tin 57.81%.
Keywords:ore-forming  fluid cassiterite  rough selection  of shaking  table W-Sn  separation
点击此处可从《中国矿业》浏览原始摘要信息
点击此处可从《中国矿业》下载全文