A low temperature route to prepare LaFeO3 and LaCoO3
Authors:AD Jadhav  V Samuel
Affiliation:a Physical and Materials Chemistry Division, National Chemical Laboratory, Pune 411008, India
b Centre for Materials Characterization, National Chemical Laboratory, Pune 411008, India
c Catalysis Division, National Chemical Laboratory, Pune 411008, India
Abstract:A combination of digestion and further low temperature calcination to crystallize the product was employed to prepare LaFeO3 (LF) and LaCoO3 (LC) powders. Freshly co-precipitated lanthanum and ferric (or cobalt) hydroxide gels by sodium hydroxide were allowed to react at 100 °C under refluxing and stirring conditions for 4-6 h. These oven dried powders were heated at 450 °C to form crystalline LF (or LC) powders. The phase contents and lattice parameters were investigated by X-ray diffraction (XRD). Transmission electron microscope (TEM) investigations were carried out to examine the morphology and average particle size of these powders.
Keywords:Chemical synthesis  X-ray diffraction  Transmission electron microscopy  Precipitation  LaFeO3
本文献已被 ScienceDirect 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号