Limit load and J estimates of a centre cracked plate with an asymmetric crack in a mismatched weld
Affiliation:1. Department of Civil, Environmental and Mechanical Engineering, University of Trento, Trento I-3812, Italy;2. Mechanics Division, National Technical University of Athens, Zographou GR-15773, Greece;3. Mechanical Engineering & Mechanics Department, Drexel University, Philadelphia, PA 19104, USA
Abstract:The limit load and J estimates of a centre cracked plate with an asymmetric crack in the tensile properties mismatched weld were investigated. A limit load expression was derived on the basis of a simplified slip-line field. A good agreement between the predictions of the expression and finite element (FE) results was found for ratios of half-weld width to the crack ligament, H/l, of less than 0.5. The equivalent stress–strain relationship method (ESSRM) was used to predict elastic–plastic J values. Results from FE analyses show that the ESSRM is accurate for the crack with asymmetry in the mismatched weld provided an accurate theoretical or numerical value of the limit load of the same specimen is available. Defect assessment methods are discussed, and it is found that the failure assessment diagram (FAD) of an asymmetrically cracked mismatched weld can be constructed from the equivalent stress–strain relationship for the same mismatched geometry with a symmetric crack. The effect of an asymmetric crack on the FAD may then be covered by the limit load solution for the asymmetrically cracked mismatched weld.
Keywords:
本文献已被 ScienceDirect 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号