再生塔底重沸器的腐蚀和对策
引用本文:王秋灵. 再生塔底重沸器的腐蚀和对策[J]. 腐蚀与防护, 2004, 25(10): 432-433,437
作者姓名:王秋灵
作者单位:中国石油化工股份有限公司洛阳分公司,洛阳,471012
摘    要:分析了气体脱硫装置再生塔底重沸器腐蚀原因主要是CO2引起的,设备结构不合理和冲蚀也是重要原因。采取了重沸器形式改进、材质升级、溶剂净化和工艺条件优化等防腐蚀措施,取得了明显效果。

关 键 词:脱硫装置  再生塔  重沸器  腐蚀  对策
文章编号:1005-748X(2004)10-0432-02

CORROSION AND COUNTERMEASURES OF REBOILER IN REGENERATOR
WANG Qiu-ling. CORROSION AND COUNTERMEASURES OF REBOILER IN REGENERATOR[J]. Corrosion & Protection, 2004, 25(10): 432-433,437
Authors:WANG Qiu-ling
Abstract:The causes of corrosion of the bottom reboiler of solvent regenerator in a gas desulfurization unit were analyzed. The carbon dioxide in the solvent, inappropriate equipment construction and erosion were the major factors resulting in corrosion. The corrosion prevention measures, including equipment construction retrofit, upgrading materials, solvent purification and process condition optimization were proposed. Good results have been obtained.
Keywords:Desulfurization unit  Regenerator  Reboiler  Corrosion  Countermeasure