作者单位:中国石油宁夏石化公司,宁夏,银川,750024
摘    要:以管线焊缝裂纹的处理为例,简要分析了18Cr-10Ni-Ti型奥氏体不锈钢焊接过程中产生裂纹的原因,提出了有针对性的防范措施,可为同类18Cr-10Ni-Ti型奥氏体不锈钢施工提供有益的借鉴。

关 键 词:18Cr-10Ni-Ti型奥氏体不锈钢  焊接裂纹  焊接工艺  防范措施

Weld cracking causes and preventive measures of 18Cr-10Ni-Ti-type austenitic stainless steel
CHANG Kehong. Weld cracking causes and preventive measures of 18Cr-10Ni-Ti-type austenitic stainless steel[J]. Petrochemical Industry Application, 2010, 29(6): 104-106
Authors:CHANG Kehong
Abstract:In this paper,an example of weld cracks in pipeline,a brief analysis of the 18Cr- 10Ni-Ti-type austenitic stainless steel during welding cracks,and proposes a targeted preventive measures for similar 18Cr-10Ni-Ti-type austenitic stainless steel construction to provide useful lessons.
Keywords:18Cr-10Ni-Ti-type austenitic stainless steel  welding cracks  welding process  preventive measures