1Cr18Ni9Ti荒管内折和纵向裂纹缺陷剖析
引用本文:王俊琴,王辉绵,白晋钢,韩载华. 1Cr18Ni9Ti荒管内折和纵向裂纹缺陷剖析[J]. 山西冶金, 1999, 0(3)
作者姓名:王俊琴  王辉绵  白晋钢  韩载华
摘    要:阐述了影响1Cr18Ni9Ti管坯热穿孔工艺性能的因素,剖析了不锈钢荒管产生内折和纵裂的原因,提出了防止上述缺陷的措施。

关 键 词:1Cr18Ni9Ti  内折  纵裂  措施

Analyzing The Defectives Of 1Cr18Ni9Ti Is Folding Inside and Longitudinal Cracks on Surface
Abstract:In this paper,it was studied that the reason of causing defectives workmanship that is folding and longitudinal cracks inside surface of stainless steel tube in lCr18Ni9Ti hot piercing and the ways of preventing above defectives was offered.
Keywords:1Cr18Ni9Ti  inside folding  longitudinal cracks  measures  