首页 | 本学科首页   官方微博 | 高级检索  
     

某氰化尾渣浮选提金试验研究
引用本文:许国璋.某氰化尾渣浮选提金试验研究[J].黄金,2019,40(7):75-78.
作者姓名:许国璋
作者单位:灵宝黄金集团股份有限公司
摘    要:以四川某金矿氰化尾渣为研究对象,针对其载金矿物和脉石矿物单一,金品位高(2.40g/t),载金矿物被氰化物强烈抑制及轻度泥化等特点,确定采用浮选法回收金。经过单因素条件试验确定最佳工艺条件,即磨矿细度-0.074mm占65%,硫酸用量350g/t,水玻璃用量250g/t,丁基黄药+丁铵黑药用量(150+75)g/t,经过一次粗选、一次精选、两次扫选闭路试验流程,获得了金品位为94.88g/t、金回收率为89.68%的金精矿。

关 键 词:氰化尾渣  浮选    硫酸  捕收剂

Experimental study on the flotation of gold from certain cyanide tailings
Xu Guozhang.Experimental study on the flotation of gold from certain cyanide tailings[J].Gold,2019,40(7):75-78.
Authors:Xu Guozhang
Affiliation:(Lingbao Gold Group Company Ltd.)
Abstract:Taking the tailings of a gold mine in Sichuan Province after cyanide heap leaching as the research object,which are characterized by single gold-bearing minerals and gangue minerals,high gold grade(2.40 g/t),gold-bearing minerals being strongly inhibited by cyanide for gold and light argillization,the study adopted flotation for gold extraction and single-factor condition test to decide optimum process parameters:grinding fineness is 65 %-0.074 mm, sulfuric acid dosage is 350 g/t,sodium silicate dosage is 250 g/t,butyl xanthate+ammonium butylene dosage is (150+75) g/t.Through a once roughing,once cleaning,twice scavenging closed circuit flowsheet,a flotation gold concentrate with gold grade 94.88 g/t and recovery 89.68 % was obtained.
Keywords:cyanide tailings  flotation  gold  sulfuric acid  collector
本文献已被 CNKI 维普 万方数据 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号