摘    要:采用光学显微镜、示差扫描热分析、交流磁化率测试和室温压缩试验等方法系统研究Ti含量对Ni53Mn23.5Ga23.5-xTix (x=0, 0.5, 2, 3.5, 8, 15)合金的显微组织、相变行为、力学行为和磁学特性的影响规律。结果表明:Ti元素在合金中的极限固溶度低于15%;随着Ti含量的增加,合金的相变温度和断裂强度及断裂应变先逐渐增加后降低,其断裂方式由沿晶断裂转变为穿晶断裂再到沿晶断裂;而合金的居里温度随Ti含量的增加逐渐降低

关 键 词:Ni53Mn23.5Ga23.5-xTix合金  铁磁性形状记忆合金  磁性能  力学性能
收稿时间:2009/9/25 0:00:00

Effect of the Ti Content on Microstructure and Properties of Ni53Mn23.5Ga23.5-xTix Ferromagnetic Shape Memory Alloy
Dong Guifu,Li Xuehui,Li Yanqin,Bu Decai,Liu Zhisheng,Cai Wei,Gao Zhiyong and Sui Jiehe.Effect of the Ti Content on Microstructure and Properties of Ni53Mn23.5Ga23.5-xTix Ferromagnetic Shape Memory Alloy[J].Rare Metal Materials and Engineering,2010,39(10):1785-1789.
Authors:Dong Guifu  Li Xuehui  Li Yanqin  Bu Decai  Liu Zhisheng  Cai Wei  Gao Zhiyong and Sui Jiehe
Affiliation:Dalian University, Dalian 116622, China;Dalian University, Dalian 116623, China;Dalian University, Dalian 116624, China;Dalian University, Dalian 116625, China;Dalian University, Dalian 116626, China;Dalian University, Dalian 116627, China;Harbin Institute of Technology, Harbin 150001, China;Harbin Institute of Technology, Harbin 150001, China
Abstract:The effect of the Ti content on polycrystalline microstructure, phase transformation behavior, mechanical behavior and magnetic properties of the Ni53Mn23.5Ga23.5-xTix (x = 0, 0.5, 2, 3.5, 8, 15, at%) ferromagnetic shape memory alloy was studied by means of OM, DSC, room temperature compression tests and ac susceptibility measurements. The results show that the solubility limit of Ti element in the alloys is below 15%. The transformation temperature, the fracture strength and the fracture strain increase at first and then decrease with increasing of the Ti content. Furthermore, it is concluded that Ti addition can change the fracture type of Ni53Mn23.5Ga23.5-xTix alloys from the intergranular fracture to the transgranular to the intergranular again. In addition, the Curie temperature decreases gradually with the increase of Ti content in Ni53Mn23.5Ga23.5-xTix alloys
Keywords:Ni53Mn23  5Ga23  5-xTix (x=0  0  5  2  3  5  8  15) alloy  ferromagnetic shape memory alloy  magnetic properties  mechanical properties