某贫硫金矿无捕收剂浮选的试验研究
引用本文:刘建业,刘杰,张淑敏. 某贫硫金矿无捕收剂浮选的试验研究[J]. 有色矿冶, 2010, 26(5): 20-23
作者姓名:刘建业  刘杰  张淑敏
作者单位:[1]辽宁省矿产勘查院,辽宁沈阳110031 [2]东北大学资源与土木工程学院,辽宁沈阳110004
摘    要:针对某地贫硫石英脉含金矿石,采用无捕收剂浮选工艺,在原矿金品位4g/t,磨矿细度-0.074mm占65%、硫化钠用量300g/t,2#油用量168.8g/t、丁基黄药用量4g/t、浮选时间16min的情况下,可获得金精矿品位30.11g/t、回收率94.63%的技术指标。

关 键 词:贫硫金矿  无捕收剂  浮选

Study on Collectorless Flotation of the Poor Sulfide Gold Ore
LIU Jian-ye,LIU Jie,ZHANG Shu-min. Study on Collectorless Flotation of the Poor Sulfide Gold Ore[J]. Non-Ferrous Mining and Metallurgy, 2010, 26(5): 20-23
Authors:LIU Jian-ye  LIU Jie  ZHANG Shu-min
Affiliation:1.Liaoning Mining Exploration Survey Institue,Shenyang 110031,China;2.School of Resources and civil Engineering,Northeastern university,Shenyang 110004,China)
Abstract:Collectorless flotation process for poor sulfide gold ore in quartz vein was studied under such conditions as gold grade of run -of mine ore 4 g/t,grinding fineness(-0.074 mm) 65%,flotation agent as sodium sulfide 300 g/t,2# oil 168.8 g/t and butyl xanthic acid 4 g/t,flotation time 16 min,etc..And the concentrate with gold grade of 30.11 g/t and recovery of 94.63% were achieved.
Keywords:Collectorless  poor sulfide gold ore  flotation