摘    要:用Thermomacmaster-Z热模拟机和TEM,SEM研究了G3(%:0.012C、46.51Ni、24.71Cr、8.88Mo、1.15W、1.72Cu、0.10Nb)、G3-Z(%:0.014C、46.53Ni、24.05Cr、6.89Mo、1.09W、1.70Cu)和825耐蚀合金(%:0.006C、43.77Ni、22.10Cr、3.24Mo、1.90Cu、0.86Ti)1 030~1 300℃、应变量(ε)0~0.8、应变速率1~2.5 s-1的应力-应变曲线和温度对合金最大应力和断面收缩率的影响,并分析了合金发生动态再结晶的影响因素。结果表明,G3、G3-Z、825合金动态再结晶的晶粒大小随温度补偿系数Z的增大而减小;G3、G3-Z、825合金适宜的热加工温度范围分别为1 100~1 240℃、1 130~1 220℃和1 050~1 240℃。

关 键 词:G3、G3-Z  825耐蚀合金  应力-应变  热塑性  
收稿时间:2009-03-11

A Study on Hot Workability of Corrosion Resistance Alloy G3,G3-Z and 825
Bao Yaozong,Dong Han,Su Jie,Yong Qilong,Wang Lihui,Li Mingzhi.A Study on Hot Workability of Corrosion Resistance Alloy G3,G3-Z and 825[J].Special Steel,2009,30(5):1-3.
Authors:Bao Yaozong  Dong Han  Su Jie  Yong Qilong  Wang Lihui  Li Mingzhi
Affiliation:1. Institute for Structure Materials,Central Iron and Steel Research Institute,Beijing 100081; 2. Xinxing Cast Pipe Group Co.Ltd,Handan 056000; 3. Oil Production Engineering Technology Institute,Zhongyuan Oil-field Branch Co,Puyang 457001;
Abstract:The stress-strain curves of corrosion resistant alloys G3 (%:0.012C,46.51Ni,24.71Cr,8.88Mo, 1.15W,1.72Cu,0. 10Nb),G3-Z(%:0.014C,46.53Ni,24.05Cr,6.89Mo,1.09W,1.70Cu)and alloy 825(%: 0.006C,43.77Ni,22. 10Cr,3.24Mo,1.90Cu,0.86Ti) with strain(e)0~0.8,strain rate 1~2.5s-1 at 1030~ 1300 ℃ and the effect of temperature on max stress and reduction of area of alloys have been studied by using Thermomac-master-Z hot simulator,TEM and SEM,and the effect factors on dynamic recrystallization of alloys were analyzed. Results showed that with increasing temperature compensating factor Z,the grain size of dynamic-crystallizing of alloy G3,G3-Z and 825 decreased,and the available temperature range for hot-working was 1100~1240 ℃ for alloy G3,1130~1220 ℃ for alloy G3-Z and 1050~1240 ℃ for alloy 825.
Keywords:Corrosion Resistant Alloy G3  G3-Z  825  Stress-Strain  Hot Ductility  