摘    要:提出两段氧化—碱浸—酸浸工艺来回收改性含钛高炉渣中的铁、钒和钛.较佳的提铁实验条件为一段氧化时间40 s和保温时间8 min,铁的回收率为89.93%.较佳的提钒实验条件为总氧化时间126 s、NaOH浓度4.0 mol/L、浸出温度95℃、浸出时间90 min和碱浸循环次数4,钒的浸出率为92.13%.较佳的提钛实验...

关 键 词:含钛高炉渣  氧化  改性  浸出  人造金红石  生铁
收稿时间:20 December 2020

Recovery of Fe,V,and Ti in modified Ti-bearing blast furnace slag
Ji-qing HAN,Jing ZHANG,Jia-hao ZHANG,Xiao CHEN,Li ZHANG,Gan-feng TU.Recovery of Fe,V,and Ti in modified Ti-bearing blast furnace slag[J].Transactions of Nonferrous Metals Society of China,2022,32(1):333-344.
Authors:Ji-qing HAN  Jing ZHANG  Jia-hao ZHANG  Xiao CHEN  Li ZHANG  Gan-feng TU
Affiliation:(School of Metallurgy,Northeastern University,Shenyang 110819,China;School of Materials Science and Engineering,Northeastern University,Shenyang 110819,China)
Abstract:A two-stage oxidation—alkali leaching—acid leaching method was proposed to recovery Fe, V, and Ti in modified Ti-bearing blast furnace slag. The optimal experiment conditions of iron extraction were one-stage oxidation time 40 s and holding time 8 min. The recovery rate of iron was 89.93%. The optimum experiment conditions of vanadium extraction were total oxidation time of 126 s, NaOH concentration of 4.0 mol/L, leaching temperature of 95 °C, leaching time of 90 min, and the number of cycle was 4. The leaching rate of vanadium was 92.13%. The optimal experiment conditions of titanium extraction were HCl concentration of 4.5 mol/L, leaching temperature of 75 °C, and leaching time of 90 min. The TiO2 content of synthetic rutile was 98.61%.
Keywords:Ti-bearing blast furnace slag  oxidation  modification  leaching  synthetic rutile  pig iron