首页 | 本学科首页   官方微博 | 高级检索  
     

低上浆率织造用浆料的配方设计机制
引用本文:武海良,沈艳琴,姚一军,毛宁涛.低上浆率织造用浆料的配方设计机制[J].纺织学报,2016,37(12):60-64.
作者姓名:武海良  沈艳琴  姚一军  毛宁涛
作者单位:1. 西安工程大学 纺织与材料学院,陕西 西安,710048;2. 西安工程大学 纺织与材料学院,陕西 西安 710048; 英国利兹大学 设计学院,英国 利兹 LS29JT
基金项目:陕西省科学技术研究与发展计划项目(2015GY161);2014年纺织之光应用基础研究项目(J201407)
摘    要:针对目前纺织企业高上浆率织造的问题,采用不同组分的浆料配方对纯棉经纱进行上浆,系统测试了浆纱的上浆率、回潮率和力学性能,并在实际生产中进行了织造,统计了织造过程中经纱、纬纱断头次数及织造效率。通过研究共混浆料浆膜性能、浆膜的织态结构、浆料组分对浆膜织态结构和浆液相分离的影响,从理论上分析了造成各浆料配方织造效率不同的机制,指出了目前高上浆率织造的原因,提出了低上浆率条件下纯棉经纱织造的浆料配方构成机制,推荐了低上浆率工艺下实现纱线高效率织造的浆料配方,当聚乙烯醇与A115 变性淀粉质量比为37.5:62.5时,可满足低上浆率条件下织造,为印染前处理减轻负荷。

关 键 词:低上浆率  织态结构  织造  相分离  浆料配方  
收稿时间:2016-03-29

Size recipe design mechanism for low add-on weaving
Abstract:Aiming at the problem of weaving with greater sizing add-on rate in existing textile enterprise, the different size formulations wereadopted to size cotton yarns and the sizing add-on rate, moisture regain and mechanical property were tested. The sized yarnswoven in theactual production. The warp and weft stops, weaving efficiency were counted. The performance and morphological structure of sizing membranes, the influences of sizing recipe components on morphological structure of sizing membranes and phase separation of sizing solution were investigated,and it isbelieved that this might be the reason why greater add-on rate of existing sizing materials are required to meet the requirements of high speeding weaving. Based on the above analysis, the principles of design sizing recipes for high performance cotton yarns of low sizing add-on rate are proposed, and weaving processability of cotton yarns using an optimised sizing formulation composed of polyvinyl alcohol and modified starchKollotex A115 at a ratio of 37.5:62.5 for low sizing add-on rate of 5.5%~6.8% are reported to ease the burden of dyeing pretreatment.
Keywords:low size add-on  morphological structure  weaving  phase separation  size recipe
本文献已被 CNKI 万方数据 等数据库收录!
点击此处可从《纺织学报》浏览原始摘要信息
点击此处可从《纺织学报》下载全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号