Effect of Tangential Loading on Critical Conditions for Radial Cracking in Brittle Coatings
Authors:Chul-Seung Lee  Brian R. Lawn   Do Kyung Kim
Affiliation:Materials Science and Engineering Laboratory, National Institute of Standards and Technology, Gaithersburg, Maryland 20899;Department of Materials Science and Engineering, Korea Advanced Institute of Science and Technology, Yusong, Taejon 305–701, Korea
Abstract:Results of Hertzian contact tests investigating the effects of superposed tangential loads on the critical conditions for radial cracking at the undersurfaces of brittle coatings on compliant substrates are reported. It is demonstrated that these effects are secondary, so that conventional normal indentation remains an appropriate test procedure for characterizing this highly deleterious mode of coating fracture under a wide range of complex loading conditions.
Keywords:brittle materials    coatings    layered ceramics    cracks/cracking