1.
The structure and electrical properties of (Na0.5Bi0.5)0.94Ba0.06TiO3 ceramic doped with 0.5 wt% of MnO were investigated in comparison with those of (Na0.5Bi0.5)0.94Ba0.06TiO3 ceramic. It was ascertained that the MnO addition did not cause remarkable change in crystal structure and microstructure. The MnO addition mainly displayed a hard effect on the electrical properties, an increase of coercive field (E) and mechanical quality factor (Qm) together with a decrease of dielectric constant (εr) and piezoelectric constant (d33). An enhancement of electromechanical coupling factor (kp) with the MnO addition was obtained too. An essential relation between the piezoelectric properties and ferroelectric nature of the ceramics was detected. It was found that the piezoelectric properties of the ceramics highly depended on the corporative contribution of remanent polarization (Pt) and coercive field.  相似文献   

2.
MgO-modified Li0.06(Na0.5K0.5)0.94NbO3(L6NKN) lead-free piezoelectric ceramics were synthesized by normal sintering at a relatively low temperature of 1000°C.The crystalline phase,microstructure,and electrical properties of the ceramics were investigated with a special emphasis on the influence of MgO content.The addition of MgO effectively improves the sinterability of the L6NKN ceramics.X-ray diffraction analysis indicates that the morphotropic phase boundary(MPB) separating orthorhombic and tetragonal ph...  相似文献   

3.
Bi0.5Na0.5TiO3系无铅压电陶瓷的研究   总被引:5,自引:0,他引:5  
概述了Bi0.5Na0.5TiO3(BNT)基无铅压电陶瓷的研究近况。第二组元化合物的加入能使BNT陶瓷的矫顽场降低,使BNT基陶瓷的压电性能得到了提高。根据BNT基无铅压电陶瓷的A位和B位原子的原子量、离子半径和电负性,研究了BNT基压电陶瓷的性能与这些参数的关系。  相似文献   

4.
1INTRODUCTION Therehasbeengreatinterestinthestudiesof thelead freematerialswithdielectric,piezoelectricandferroelectricpropertiesinthefieldoffunction almaterialsfortheiramiabilitytoenvironment. (Na1/2)TiO3(NBT)ceramicshavebeenwidelystudiedbecauseoftheirrelativelylargeremnant polarization(Pr)of38μC/cm2andcoercivefieldof 73kV/cm[1].However,NBTcannotreplacelead zirconatetitanate(PZT)basedceramicsbecausethepiezoelectricpropertiesofNBTarestillnot comparabletothoseofPZT[24].Recently,m…  相似文献   

5.
本文采用传统陶瓷工艺,制备得到Bi0.5(Na1-x-yKxLiy)0.5TiO(3简称BNKLT)无铅压电陶瓷,运用X射线衍射、扫描电子显微镜对其进行了分析表征;通过压电、介电性能的对比,讨论了烧结温度对BNKLT陶瓷的影响;运用热分析及X射线衍射等手段,确定了粉体的热处理温度,并讨论了烧结温度对BNKLT陶瓷性能的影响;通过最终所得陶瓷的性能对比,确定制备的较优工艺参数。  相似文献   

6.
采用溶胶-凝胶法制备工艺制备了(1-x)(Na0.5Bi0.5)TiO3-xBa0.092Ca0.03Sr0.05TiO3(x=0.04、0.06、0.07、0.08)系无铅压电陶瓷。研究了陶瓷的铁电、压电性能和显微结构。结果表明,该体系陶瓷在x=0.06时,其压电常数d33,机电耦合系数kp,厚度耦合系数kt,相对介电常数rε,介质损耗tgδ,分别为152,0.24,0.47,1 250,0.04。  相似文献   

7.
Ferroelectric Ba0.7Sr0.3TiO3(BST) and partially Pb2+ substituted for Ba2+ ceramics (Bao.7-xPbx)Sr0.3TiO3 (x=0.1-0.4,BPST) were prepared by using conventional solid-reaction method.XRD analysis shows that the samples microstructure changes from cubic phase to tetragonal one with the Pb2+ content increasing.ESEM analysis shows that the Pb2+ substituted samples have a denser and more uniform surface morphology than that of pure BST.Measured electrical properties suggest that the Pb2+ substitution for Ba2+ in the BST system enhances the ferroelectric performance obviously when x=0.2.In addition,the substitution increases the samples Curie temperature (Tc).(Ba0.5Pb0.2)Sr0.3TiO3 ceramic has good ferroelectric properties measured at a maximal electric field of 30 kV/cm under the condition of room temperature.The corresponding saturated polarization (Ps),remnant polarization (Pr) and coercive field (Ec) is respectively 15.687 μC/cm2,8.100μ C/cm2 and 6.611 kV/cm.The measured Tc of (Ba0.5Pb0.2)Sr0.3TiO3 is 117 ℃.  相似文献   

8.
为了改善无铅压电陶瓷介电性能,采用传统陶瓷制备方法,制备一种新型Bi基钙钛矿型三元系无铅压电陶瓷(1-x-y)BNT-xBKT-yBiFeO3,并研究极化对该体系陶瓷介电性能的影响以及介电性能随频率的变化规律。结果表明:极化后的介电常数和介电损耗低于极化前。极化前的介电常数和介电损耗随BiFeO3含量的增加变化不明显,极化后的介电常数和介电损耗随BiFeO3含量的增加而增加。极化前和极化后的介电常数和介电损耗随BKT含量的增加而增加。介电常数和介电损耗随频率增加分别降低和增加,但降低和增加速率随频率增加而降低。  相似文献   

9.
采用传统的固相烧结法于1120℃烧结2 h得到(0.82-x)Bi0.5Na0.82Ti O3-0.18Bi0.5K0.18TiO3-xBiFeO3(x=0.01-0.07)无铅压电陶瓷,并对该体系陶瓷的微观结构和电学性能进行了研究。结果表明,BiFeO3的引入量x为0.01-0.07时,样品均为具有MPB准同型相界(三方相和四方相共存)的钙钛矿结构。BiFeO3的引入使陶瓷的晶粒度略有增加;当x=0.03时,样品达到最大致密度。为97.7%;陶瓷的压电常数d33随BiFeO3的引入而降低。陶瓷的相对介电常数εr和居里温度随BiFeO3的引入而明显增大,在x=0.03时达到最大值。  相似文献   

10.
为了抑制K_(0.5)Bi_(0.5)TiO_3的退极化现象,提高铁电性能,以K_2CO_3、TiO_2、Bi_2O_3及ZnO为原料,通过二步固相法合成无铅铁电复合陶瓷K_(0.5)Bi_(0.5)TiO_3:ZnO(KBT:ZnO).通过X射线衍射、扫描电子显微镜、铁电和介电测试分析了复合陶瓷的微观结构和介电行为.结果表明:KBT中引入20%(物质的量百分数)的ZnO后,复合陶瓷中生成了第三相Zn2TiO_4,同时,KBT的极化能力及其铁电行为得到改善.阻抗测试表明复合铁电陶瓷内部只存在一种导电机制,即电子电导.特别是ZnO的引入抑制了KBT由正常铁电体向弛豫铁电体的相转变,对KBT的应用和研究有着重要的作用.  相似文献   

11.
无铅压电陶瓷的研究与进展   总被引:7,自引:0,他引:7  
无铅压电陶瓷是当前压电铁电领域的研究热点之一。结合近期国内外有关无铅压电陶瓷方面的论文和发明专利,综合分析了无铅压电陶瓷研究和开发的相关进展,着重给出了无铅压电陶瓷主要种类的相关体系及压电铁电性能。  相似文献   

12.
Lead-free piezoelectric (K0.5sNa0.5)1-xLixNbO3 (x = 0at%-20at%) ceramics were synthesized by spark plasma sintering (SPS) at low temperature and the effects of LiNbO3 addition on its crystal structure and properties were also studied. When the Li content was less than 6at%, a single proveskite phase with the similar structure of (K0.5Na0.5)NbO3 was formed; and a secondary phase with K3Li2Nb5O15 structure was observed in the 6at% 〈 x 〈 20at% compositional range. Furthermore, LiNbO3 existed as the third phase when the Li content was higher than 8at%. The grain sizes increased from 200-500 nm to 5-8 μm when the K3Li2Nb5O15 and LiNbO3 like phases were formed. With increasing Li content, the relative density of the ceramics first decreased from 97% to 93% and then kept constant. The piezoelectric coefficient d33, dielectric constant, and planner electromechanical coupling factor exhibited a decreasing tendency with increasing Li content because of the decrease in density and the formation of the secondary phase such as K3Li2Nb5O15 and LiNbO3. The formation of dense microstructure with a single phase is necessary in improving the properties of the (K0.5Na0.5)1-xLixNbO3 ceramics.  相似文献   

13.
Manganese-doped Ba_(0.925)Ca_(0.075)TiO_3 lead-free piezoelectric ceramics(abbreviated as BCT)with high mechanical quality factor were synthesized by conventional solid-state reaction method.The effects of excess Ba on the crystal structure,microstructure,and electrical properties of the ceramics were systematically investigated.X-ray diffraction and Raman spectra revealed that Ca~(2+)ions were pushed from Ba sites to Ti sites of BCT when 1.5 mol%extra Ba~(2+)ions were added after sintering.The grain size of the ceramics was decreased by adding extra Ba~(2+)ions.The mechanical quality factor and resistivity of the ceramics decreased dramatically when the excess Ba was more than 1.5 mol%.High piezoelectric coefficients(d_(33)=150-190 pC/N)and high mechanical quality factors(Q_m=1 000-1 200)were obtained in the ceramics when the excess of Ba was between 0.5 mol%and 1 mol%.These results indicated that the properties of BCT ceramics could be tailored by adjusting the content of Ba.  相似文献   

14.
采用传统陶瓷工艺方法制备了La2O3掺杂(Bi1/2Na1/2)0.94Ba0.06TiOa(BNBT6)无铅压电陶瓷,系统地研究了La2O3掺杂对该体系陶瓷介电、压电性能与微观结构的影响.结果表明:该体系具有很高的压电常数,是单一的钙钛矿结构,La2O3的添加对晶粒生长具有一定的抑制作用,线收缩率和相对密度增大.室温介电常数随着La2O3掺杂量的增加而增大.与不添加La2O3的陶瓷样品相比,添加少量La2O3可以使体系的弛豫特征更为明显.当掺杂量为0.1 wt%时,该体系陶瓷具有较好的综合性能:d3a=160 pC/N,kp=0.322.当掺杂量达到0.5 wt%以后,陶瓷的压电性能严重降低.  相似文献   

15.
The microstructures and electrical properties of Bi0.5(Na1-x-yKxLiy)0.5TiO3 lead-free piezoelectric ceramics were studied.These ceramics were prepared by conventional ceramic technique.XRD analysis reveals that the ceramics possess almost pure perovskite phase when y≤0.2.The SEM results show that,with more amounts of Li+,the crystalline grain growing speed is accelerated,and the sintering temperature can effectively be decreased.The measurements of piezoelectric properties indicate that the ceramics with relatively low amount of Li+ and high amount of K+ have comparatively large piezoelectricity.The dielectric measurements show that the ceramics have properties like relaxor ferroelectrics and diffuse phase transition(DPT) at Td and Tc,respectively.The results of ferroelectric measurements reveal the system has relatively higher remanent polarization Pr(27.6 μC/cm2) and lower coercive field Ec(37.5 kV/cm).  相似文献   

16.
planarelectromechanicalcouplingfactor;piezoelectricchargeconstant1Introduction Leadoxide basedpiezoelectricceramics,suchasPb(Ti,Zr)O3(PZT),arenowwidelyusedinvariousappli cationssuchastransducers,filters,oscillatorsandactua torsbecauseoftheirsuperiorpiezoe…  相似文献   

17.
针对目前无铅压电陶瓷的压电常数d33偏小的情况,采用传统的烧结方法制备了(Na0.5K0.5)NbO3基无铅压电陶瓷(Na0.5K0.45Li0.05)Nb0.95-xSbxTa0.05O3(x=0.03,0.06,0.09,0.12),研究了在Li和Ta含量固定的情况下,Sb元素的添加量和烧结温度对陶瓷的压电常数的影响.研究结果表明,适量Sb元素的掺杂可以大幅度提高陶瓷的压电常数d33,陶瓷样品的压电常数d33随着Sb含量的增加先增大后减小.烧结温度可以影响陶瓷的密度,进而影响其压电常数.在1130℃的最佳烧结温度下,Sb含量x=0.09时,陶瓷样品表现出最佳的压电性能,压电常数d33=328 pC/N.  相似文献   

18.
A new group of lead-free piezoelectric ceramics,(Bi0.5 Na0.5)1-x(BaaSrb)xTiO3(abbreviated as BNBST[100x-100a/100b],0〈x〈1,a+b=1),was synthesized.The ceramics were prepared by conventional ceramic sintering technique,and the ceramics with density of 95% of the theoretical one can be sintered without the atmosphere control during the sintering process.The results of the X-ray diffraction(XRD) data show that the ceramics possess a single perovskite phase.The measurements of dielectric and piezoelectric properties reveal that the ceramics provide relatively high piezoelectric charge constant d33 and high planar electromechanical coupling factor kp.For the BNBST6-95/5 ceramics,d33 is equal to 170pC/N,and kp is equal to 32.0%.The fabrication technique for these ceramics is conventional and stable.  相似文献   

19.
采用凝固法制备出各向异性的片状钛酸钡作为模板,利用模板晶粒生长(TGG)法制备出Na0.5K0.5NbO3(NKN)织构化陶瓷.研究了NKN织构化陶瓷的工艺、组织和性能.研究结果表明,钛酸钡可以作为NKN陶瓷的模板,在陶瓷烧结过程中诱导NKN晶粒的生长,模板的取向决定了NKN陶瓷晶粒取向,随着烧结温度的升高陶瓷的压电性能(d33)达到69 pC/N,在合理的烧结工艺下得到了取向比较明显的织构化陶瓷.  相似文献   

20.
Manganese-doped Ba0.925Ca0.075TiO3 lead-free piezoelectric ceramics (abbreviated as BCT) with high mechanical quality factor were synthesized by conventional solid-state reaction method. The effects of excess Ba on the crystal structure, microstructure, and electrical properties of the ceramics were systematically investigated. X-ray diffraction and Raman spectra revealed that Ca2+ ions were pushed from Ba sites to Ti sites of BCT when 1.5 mol% extra Ba2+ ions were added after sintering. The grain size of the ceramics was decreased by adding extra Ba2+ ions. The mechanical quality factor and resistivity of the ceramics decreased dramatically when the excess Ba was more than 1.5 mol%. High piezoelectric coefficients ( d33 = 150–190 pC/N ) and high mechanical quality factors ( Qm = 1 000–1 200 ) were obtained in the ceramics when the excess of Ba was between 0.5 mol% and 1 mol%. These results indicated that the properties of BCT ceramics could be tailored by adjusting the content of Ba.  相似文献   