The flow stress features of MB26 magnesium alloy were studied by isothermal compression at 300-450 ℃ and strain rate of 0.001^-1 s J with Gleeble 1500 thermal simulator. In addition, the deformation activation energy Q was calculated. The results show that the strain rate and deformation temperature have obvious effect on the true stress. The peak value of flow stress becomes larger with increasing strain rate at the same temperature, and gets smaller with the increasing deformation temperature at the same strain rate. The alloy shows partial dynamic recrystallization. The flow stress of MB26 magnesium alloy during high temperature deformation can be represented by Zener-Hollomon parameter including the Arrhemius term. The temperatt, re range of 350-400℃ is suggested for hot-forming of this alloy.  相似文献   
2.
采用红外辐射热冲击加热的瞬态气动加热系统对Al-Mg-Li合金进行快速加热,研究快速加热对Al-Mg-Li合金高温力学性能和组织的影响.结果表明:采用该加热系统40 s可以达到温度场均匀,在150℃时Al-Mg-Li合金的屈服强度和抗拉强度分别为300MPa、380MPa,是室温强度的80%以上,具有良好的高温性能;Al-Mg-Li合金良好的高温强度不仅与δ粒子重新回复有序结构有关,而且与高温下δ粒子长大提高合金的时效强化有关.  相似文献   
1
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号