 共查询到20条相似文献,搜索用时 563 毫秒
1.
以铁矿石为主要原料,通过煅烧酸浸法制备出硫酸铁,再以硫酸铁、硅酸钠和四硼酸钠为原料,制备了无机高分子混凝剂含硼聚硅硫酸铁(PFSSB)。研究了PFSSB的制备工艺条件以及PFSSB投加量和废水pH对PFSSB的混凝效果的影响。结果表明:当二氧化硅质量分数为3%、活化时间为40 min、活化pH为3、铁与硅物质的量比为0.50、硼与硅物质的量比为0.50时,得到的PFSSB具有最好的性能,用其处理高COD、高浊度工业废水,混凝效果明显优于聚合硫酸铁(PFS)。  相似文献   

2.
含硼聚硅硫酸铁的制备及絮凝效果研究   总被引:1,自引:0,他引:1  
以硅酸钠、硫酸铁和四硼酸钠为原料,制备了无机高分子絮凝剂含硼聚硅硫酸铁(PFSSB),研究了PF—SSB的制备工艺条件、PFSSB投加量和废水pH对PFSSB絮凝效果的影响。结果表明,当制备工艺条件为:二氧化硅质量分数为3%,活化时间为30min,活化的pH为3,铁与硅物质的量比为0、50,硼与硅物质的量比为0.40时,得到的PFSSB具有最好的性能,用其处理高COD、高浊度工业废水,絮凝效果明显优于聚合硫酸铁(PFS)。  相似文献   

3.
无机高分子絮凝剂作为一类新型水处理剂近年来得到了快速发展。采用硅酸钠、硫酸铁等为原料,制备了聚硅硫酸铁(PFSS)絮凝剂,并以印染废水为对象对其絮凝效果进行了研究。主要考察了SiO2浓度、Fe/Si物质的量比、聚硅酸(Ps)活化时间、聚硅酸(PS)与聚硫酸铁(PFS)聚合温度、聚合pH值等因素对产品絮凝性能的影响。结果表明,在SiO2浓度为1.096、Fe/Si物质的量比为0.5、聚硅酸(PS)活化时间为3h、聚硅酸(PS)与聚硫酸铁(PFS)聚合温度为60℃,聚合pH值为1.5条件下制备的聚硅硫酸铁对废水絮凝效果最好,浊度脱除率达到88.9%,废水的COD去除率达到80.9%。  相似文献   

4.
新型混凝剂含硼聚硅硫酸铁的性能研究   总被引:11,自引:0,他引:11  
本文制备了一种新型高分子混凝剂含硼聚硅硫酸铁 (PFSSB) ,考察了体系中硼量及铁量对其性能的影响 ,并探讨了其混凝特性和混凝机理。结果表明 ,当体系中B与Si、Fe与Si的摩尔比分别为 0 1 6及 0 50时 ,混凝剂具有最优的混凝和稳定性能。与聚铁 (PFS)、聚硅硫酸铁 (PFSS)相比 ,PFSSB的pH适用范围更宽 (pH >6 .5) ,絮体矾花大 ,适用性更强 ,沉降性能更好 ,是一种性能优异、很有发展前景的混凝剂。混凝机理分析表明 ,该混凝剂优异的混凝性能是Fe3+ 、聚硅酸、B和SO2 -4离子相互促进协同作用的结果  相似文献   

5.
无机高分子复合絮凝剂PFSS的制备与性能研究   总被引:11,自引:0,他引:11  
郑怀礼  袁宗宣  龚迎昆 《精细化工》2002,19(8):450-452,462
研究了无机高分子复合絮凝剂聚硅硫酸铁 (PFSS)的制备与絮凝性能。通过对SiO2 的质量分数、铁硅量比、PFSS的 pH值、硅酸活化时间等因素的调整和控制 ,制备出性能优异的絮凝剂。研究结果表明 :w(SiO2 ) =1 4 %~ 2 0 % ,n(Fe)∶n(Si) =(0 8~ 1 0 )∶1 0 ,PFSS的pH =1 5~ 1 8,硅酸活化时间 1~ 18h时 ,可获得絮凝性能优异的无机高分子复合絮凝剂。将制备的絮凝剂用于实际废水样品处理 ,其除浊效果明显优于目前常用的絮凝剂PAC、PFS、FeCl3 、Fe2(SO4) 3 。  相似文献   

6.
以硅酸钠、硫酸铁、硫酸铝和硼砂为原料制备无机高分子含硼聚硅酸硫酸铝铁絮凝剂(PFASSB),最佳制备条件为:n(Fe):n(Al):n(Si)=0.5:0.5:1.0,n(B):n(Si)=0.15:1,活化pH值为2.0,活化时间为1h,PFASSB具有优良的稳定性和絮凝性能,最佳稳定时间是60d。  相似文献   

7.
以铁矿石为原料,通过煅烧酸浸法制备出硫酸铁,再以硫酸铁和硅酸钠为原料,制备了无机高分子混凝剂聚硅硫酸铁(PFSS).研究了PFSS的制备工艺条件,以及PFSS投加量和废水pH对混凝效果的影响.研究结果表明:用PFSS处理工业废水,其对废水COD、浊度、色度的去除率明显好于聚合硫酸铁(PFS).PFSS适宜的制备工艺条件:二氧化硅质量分数为3%,硅酸活化时间为40 min,硅酸活化pH为2,铁与硅物质的量比为0.50.  相似文献   

8.
通过正交实验研究了用盐酸、硫酸、硫铁矿烧渣和硅酸钠制备聚硅氯化硫酸铁(PSFCS)絮凝剂的工艺条件.实验结果表明,在烧渣粒度为0.18 mm、反应时间为3 h、反应温度为120℃,硫酸浓度为6 mol/L、盐酸浓度为3 mol/L、质量液固比为4∶1的条件下,铁的浸出率可达90.7%.PSFCS的合成条件为:Fe/Si摩尔比2、硅酸括化pH值2、硅酸活化时间40 min、陈化时间2.5 h.与聚合硫酸铁(PFS)和聚合氯化铝(PAC)比较了处理印染废水的效果,表明PSFCS具有良好的絮凝性能,浊度的去除率可达96.5%.  相似文献   

9.
新型复合絮凝剂在轧制乳化油废水处理中的应用   总被引:1,自引:0,他引:1  
刘红  向慧敏  方月梅  黄莺 《化学工程师》2006,20(3):54-56,63
制备了不同Al∶Si、Fe∶Si和(Al Fe)∶Si摩尔比的聚硅酸金属盐系列絮凝剂:聚硅氯化铝(PASC)、聚硅硫酸铁(PFSS)和聚硅硫酸铁氯化铝(PFASC),实验考察了成分摩尔比、废水pH值、絮凝剂投加量对除油效果的影响。结果表明:金属与硅的摩尔比对除油效率有较大的影响,最佳摩尔比为:n(Al)∶n(Si)=3∶1、n(Fe)∶n(Si)=2∶1和n(Al Fe)∶n(Si)=4∶1;废水pH值为4~10时,处理效果都较好;随着投药量的增加,油的去除率增加,PASC、PFSS和PFAS适宜的投药量(以金属离子浓度计)分别为:900mg.L-1、1100mg.L-1、800mg.L-1。用它们来处理实际废水时,效果很好,残余油量低于国家排放标准。  相似文献   

10.
《云南化工》2017,(11):29-32
研究了聚硅酸铝锌絮凝剂适宜制备条件和提高絮凝性能的适宜条件。以硅酸钠、氯化铝、氯化锌为原料,制备聚硅酸铝锌絮凝剂,处理含磷废水。结果表明,硅酸钠浓度0.5mol/L,活化p H为4,活化时间60min,n(Al)/n(Si)为2,n(Zn)/n(Si)为3,水样p H为12,静沉时间10min时,含磷废水处理效果较好,除磷率可达98.6%。  相似文献   

11.
It is well established that a wide range of drugs of abuse acutely boost the signaling of the sympathetic nervous system and the hypothalamic–pituitary–adrenal (HPA) axis, where norepinephrine and epinephrine are major output molecules. This stimulatory effect is accompanied by such symptoms as elevated heart rate and blood pressure, more rapid breathing, increased body temperature and sweating, and pupillary dilation, as well as the intoxicating or euphoric subjective properties of the drug. While many drugs of abuse are thought to achieve their intoxicating effects by modulating the monoaminergic neurotransmitter systems (i.e., serotonin, norepinephrine, dopamine) by binding to these receptors or otherwise affecting their synaptic signaling, this paper puts forth the hypothesis that many of these drugs are actually acutely converted to catecholamines (dopamine, norepinephrine, epinephrine) in vivo, in addition to transformation to their known metabolites. In this manner, a range of stimulants, opioids, and psychedelics (as well as alcohol) may partially achieve their intoxicating properties, as well as side effects, due to this putative transformation to catecholamines. If this hypothesis is correct, it would alter our understanding of the basic biosynthetic pathways for generating these important signaling molecules, while also modifying our view of the neural substrates underlying substance abuse and dependence, including psychological stress-induced relapse. Importantly, there is a direct way to test the overarching hypothesis: administer (either centrally or peripherally) stable isotope versions of these drugs to model organisms such as rodents (or even to humans) and then use liquid chromatography-mass spectrometry to determine if the labeled drug is converted to labeled catecholamines in brain, blood plasma, or urine samples.  相似文献   

12.
13.
Scentless plant bugs (Heteroptera: Rhopalidae) are so named because adults of the Serinethinae have vestigial metathoracic scent glands. Serinethines are seed predators of Sapindales, especially Sapindaceae that produce toxic cyanolipids. In two serinethine species whose ranges extend into the southern United States,Jadera haematoloma andJ. sanguinolenta, sequestration of host cyanolipids as glucosides renders these gregarious, aposematic insects unpalatable to a variety of predators. The blood glucoside profile and cyanogenesis ofJadera varies depending on the cyanolipid chemistry of hosts, and adults and larvae fed golden rain tree seeds (Koelreuteria paniculata) excrete the volatile lactone, 4-methyl-2(5H)-furanone, to which they are attracted.Jadera fed balloon vine seeds (Cardiospermum spp.) do not excrete the attractive lactone. Loss of the usual heteropteran defensive glands in serinethines may have coevolved with host specificity on toxic plants, and the orientation ofJadera to a volatile excretory product could be an adaptive response to save time.Mention of a commercial product does not consititute an endorsement by the USDA.  相似文献   

14.
15.
Vismiones and ferruginins, representatives of a new class of lypophilic anthranoids from the genusVismia were found to inhibit feeding in larvae of species ofSpodoptera, Heliothis, and inLocusta migratoria.  相似文献   

16.
2008~2009年世界塑料工业进展   总被引:4,自引:1,他引:3  
收集了2008年7月~2009年6月世界塑料工业的相关资料,介绍了2008~2009年国外塑料工业的发展情况,提供了世界塑料产量、消费量及全球各类树脂的需求量及产能情况。按通用热塑性树脂(聚乙烯、聚丙烯、聚苯乙烯、聚氯乙烯、ABS树脂)、工程塑料(尼龙、聚碳酸酯、聚甲醛、热塑性聚酯、聚苯醚)、特种工程塑料(聚苯硫醚、液晶聚合物、聚醚醚酮)、通用热固性树脂(酚醛、聚氨酯、环氧树脂、不饱和聚酯树脂)不同品种的顺序,对树脂的产量、消费量、供需状况及合成工艺、产品应用开发、树脂品种的延伸及应用的进一步扩展等技术作了详细介绍。  相似文献   

17.
建立了测定地球化学样品中包括As、Cr、Ge、V等18种微量、痕量元素的ICP-MS方法。地化试样用HF-HNO3混酸分解后,以1 1 HNO3溶解干渣。由于制样不使用盐酸,避免了Cl对As、Cr、Ge、V的质谱干扰。用国家一级地球化学标准物质GBW 07309制备溶液优化仪器工作参数,并用于校准。方法测定限(6s)为:0.007~6.4μg/g,精密度(RSD%,n=12)为:29%~9.4%,经过国家一级地球化学标准物质的分析验证,结果与标准值吻合。方法已应用于国土资源调查的试样分析。  相似文献   

18.
19.
20.