1.
以尿素为燃料,采用溶液燃烧法合成出M2P2O7:Eu3+(M=Ba,Sr,Ca)红色荧光粉。利用X射线衍射和荧光光谱研究了激活剂Eu3+对3种荧光粉晶体结构和发光性能的影响。结果表明,制得样品分别为纯相的六方晶系Ba2P2O7、正交晶系Sr2P2O7和四方晶系Ca2P2O7。光谱分析表明,M2P2O7:Eu3+(M=Ba,Sr,Ca)的激发峰位置和发射峰位置均基本相同。M1.95P2O7:0.05Eu3+(M=Ba,Ca)发射红光,其对应于5D0→7F2电偶极跃迁的612nm发射峰强度高于对应于5D0→7F1磁偶极跃迁的588nm和593nm发射峰,说明Eu3+在M2P2O7(M=Ba,Ca)基质中处于非对称格位;而Sr1.95P2O7:0.05Eu3+发射橙红光,Eu3+在Sr2P2O7基质中处于对称格位。在394nm激发下,M1.95P2O7:0.05Eu3+(M=Ba,Sr,Ca)的色度坐标分别为(0.35,0.21)、(0.24,0.15)、(0.35,0.21)。这3种荧光粉均能被394 nm紫外光和464 nm蓝光有效激发,发射红光或橙红光。  相似文献   

2.
以H3BO3作助熔剂,采用溶胶–凝胶法合成了Na2Zn Si O4:Eu3+红色荧光粉。用X射线衍射、荧光光谱分析对样品的结构及发光特性进行了表征,探讨了H3BO3助熔剂添加量和掺Eu3+量对Na2Zn Si O4:Eu3+发光性能的影响。结果表明:所得样品属于单斜晶系,样品的激发光谱主要由一系列线状谱峰组成,激发主峰为465 nm,归属于Eu3+的7F0→5D2特征跃迁。在波长为465 nm蓝光激发下发射红光,发射峰分别为578、591、613、653和701 nm,对应于Eu3+的5D0→7FJ(J=0,1,2,3,4)跃迁,发射主峰位于613 nm(5D0→7F2)处。当Eu3+和H3BO3的摩尔掺杂量分别为5%和0.8%时,样品的荧光发光强度最大。Na2Zn Si O4:Eu3+有望成为蓝光激发的白光发光二极管(w-LED)用红色荧光粉。  相似文献   

3.
用H3BO3作为助熔剂、尿素为燃料,采用燃烧法在较低的起始温度(650℃)下制备了的纳米级SrBPO5∶Sm3+红色荧光粉。研究了该荧光粉样品的相结构、形貌和发光特性。结果表明:SrBPO5∶Sm3+样品属于三方晶系,空间群为P3121;该荧光粉平均粒径为200nm、分散性较好。样品在近紫外光404nm的激发下发射红光,发射主峰位于558、596和645nm处,分别对应于Sm3+的4 G5/2→6 H5/2、4 G5/2→6 H7/2和4 G5/2→6 H9/2的跃迁;当Sm3+的最佳摩尔掺杂量为10%,对于既可作为助熔剂又是原料的H3BO3过量0.8%时,样品的发射峰强度最强。SrBPO5∶Sm3+有望成为近紫外激发的白光LED用新型红色荧光粉。  相似文献   

4.
采用固相法制备了白光LED红色荧光粉Ca0.71WO4∶Sm3+0.04,Li+0.25和Ca0.5-yWO4∶Eu3+0.25,Li+0.25,Sm3+y(y=0.00,0.02,0.04,0.06),通过X射线衍射(XRD)、荧光分光光度计以及稳态/瞬态荧光光谱仪研究了荧光粉样品的物相、Sm3+的掺杂量对荧光粉发光性能以及荧光寿命的影响.XRD分析表明,合成的样品均为白钨矿结构.荧光光谱表明,所合成的系列荧光粉均可以被近紫外光(393 nm)和蓝光(464 nm)有效激发,其发射主峰位于615nm处,归属于Eu3+的5D0→7F2跃迁.发光衰减曲线表明,Sm3+的掺杂对荧光粉Ca0.5WO4∶Eu3+0.25,Li+0.25荧光寿命没有影响.实验结果表明,在系列Ca0.5-yWO4∶Eu3+0.25,Li+0.25,Sm3+y荧光粉中Sm3+的最佳掺杂量为4%(摩尔分数).  相似文献   

5.
采用高温固相法制备了SrIn2-xO4∶xSm3+红色荧光粉,研究了荧光粉的发光特性.在410nm近紫外光激发下,SrIn2O4∶Sm3+荧光粉呈红色光发射,发射光谱主峰位于607 nm,对应sm3+的4G5/2→6H7/2跃迁发射.研究了Sm3+掺杂量对荧光粉发射强度的影响,发现随Sm3+掺杂量的增大,荧光粉的发射强度先增大、后减小;Sm3+摩尔掺杂量为0.1时,发光强度最大;能量传递对应的临界距离Rc为1.2 nm,其浓度猝灭机理为电多极相互作用.此外,添加碱金属离子A+ (A=Li,Na,K)提高了荧光粉的发射强度,且以添加Na+时效果最好.将该荧光粉与405 nm n-UV芯片组合,获得了红光发射.  相似文献   

6.
利用Sm3+作为激活剂采用高温固相法制备了LiGd1-x(MoO4)2:xSm3+(x=0,0.005,0.010,0.015,0.020,0.030,0.040,0.050,0.060,0.080,0.100)系列红色荧光材料.测量了荧光粉的X射线衍射谱、激发光谱和发射光谱.在紫外光的激发下,该荧光粉的发射光谱为峰值位于564、608、648nm的三峰谱线,其中位于648nm处的红光发射最强.监测648nm发射峰得到的材料的激发光谱为一峰值位于275nm的宽谱和主峰位于363、376、404nm的线状谱线,说明该荧光粉可被紫外光和近紫外光有效地激发.研究了Sm3+掺杂浓度对LiGd(MoO4)2:Sm3+荧光粉的各发射峰发光强度的影响,得出Sm3+的最佳掺杂量(摩尔分数)为3.0%.对浓度猝灭的原因进行了探讨,结果表明该荧光粉是一种较好的用于白光LED的红色发光材料.  相似文献   

7.
采用溶胶-凝胶法合成了适合于近紫外激发的Li2ZnSiO4∶Eu3+红色荧光粉,用X射线衍射、红外光谱和荧光光谱对样品进行了结构及发光性能表征。结果表明:合成样品为四方晶相Li2ZnSiO4晶体。样品的激发光谱由O2--→Eu3+电荷迁移带和Eu3+的离子特征激发峰组成。在波长为395nm的紫外激发下样品发射红光,发射主峰位于613nm,对应于Eu3+离子的5 D0→7 F2跃迁。随着Eu3+掺杂量的增加,其发光强度先增加后减小,Eu3+的最佳摩尔掺量为3.5%。  相似文献   

8.
BaMoO_4:Eu~(3+)红色荧光粉的制备及发光性质   总被引:2,自引:0,他引:2  
采用柠檬酸溶胶-凝胶法制备了BaMoO4:Eu3+红色荧光粉,差热(DSC) 和X射线衍射(XRD)研究结果表明,经过700 ℃高温烧结后可得到BaMoO4纯物相.粒度分析结果表明,经700 ℃烧结后样品的粒径约为 200 nm,随着烧结温度的升高,产物的粒径明显增大,当烧结温度为800 ℃时,样品的粒径约为 500 nm.分别以392 nm 的近紫外光和 462 nm 的可见光激发样品,BaMoO4:Eu3+荧光粉发红光,对应于Eu3+的4f-4f跃迁,其中以615 nm附近的5D0→7F2电偶极跃迁发光最强,当Eu3+的掺杂浓度约为25 mol %时,在616 nm处的发光强度最大.荧光粉在392 nm和462 nm的吸收分别与紫外光和蓝光LED芯片相匹配.因此,BaMoO4:Eu3+荧光粉是一种可能应用在白光LED上的红色荧光材料.  相似文献   

9.
采用高温固相法制备BaLa2WO7:Eu3+荧光粉,结果表明:BaLa2WO7晶体是属于单斜晶系结构,空间群P21/b,BaLa2WO7:Eu3+系列荧光粉可以被394 nm的近紫外光和464 nm可见光有效激发最强发射峰为620 nm的红光,属于Eu3+离子的5D0→7F2跃迁,并且当Eu3+的掺杂浓度为9%,焙烧温度为1300℃时荧光粉的发光性能最佳。  相似文献   

10.
采用高温固相法合成了Ca2B5O9Cl:Eu2 蓝色荧光粉,并对其发光性质进行了研究.该荧光粉在近紫外370 nm激发下的发射光谱为峰值位于453 nm的宽带发射,对应了Eu2 的4f65d→4f78S7/2特征跃迁发射.监测453nm的发射峰,得到其激发光谱为250~450nm的宽带,与产生350~410nm辐射的紫外发光二极管(ultraviolet light-emitting diode,UV-LED)管芯匹配很好.当CaCl2用量为理论用量的1.1倍,H3BO3用量为理论用量的1.3倍,Eu2 掺杂浓度为6%时,蓝光发射最强.Ca2B5O9Cl:Eu2 是适合UV-LED管芯激发的白光发光二极管用高亮度蓝色荧光粉.  相似文献   

11.
It is well established that a wide range of drugs of abuse acutely boost the signaling of the sympathetic nervous system and the hypothalamic–pituitary–adrenal (HPA) axis, where norepinephrine and epinephrine are major output molecules. This stimulatory effect is accompanied by such symptoms as elevated heart rate and blood pressure, more rapid breathing, increased body temperature and sweating, and pupillary dilation, as well as the intoxicating or euphoric subjective properties of the drug. While many drugs of abuse are thought to achieve their intoxicating effects by modulating the monoaminergic neurotransmitter systems (i.e., serotonin, norepinephrine, dopamine) by binding to these receptors or otherwise affecting their synaptic signaling, this paper puts forth the hypothesis that many of these drugs are actually acutely converted to catecholamines (dopamine, norepinephrine, epinephrine) in vivo, in addition to transformation to their known metabolites. In this manner, a range of stimulants, opioids, and psychedelics (as well as alcohol) may partially achieve their intoxicating properties, as well as side effects, due to this putative transformation to catecholamines. If this hypothesis is correct, it would alter our understanding of the basic biosynthetic pathways for generating these important signaling molecules, while also modifying our view of the neural substrates underlying substance abuse and dependence, including psychological stress-induced relapse. Importantly, there is a direct way to test the overarching hypothesis: administer (either centrally or peripherally) stable isotope versions of these drugs to model organisms such as rodents (or even to humans) and then use liquid chromatography-mass spectrometry to determine if the labeled drug is converted to labeled catecholamines in brain, blood plasma, or urine samples.  相似文献   

12.
13.
建立了测定地球化学样品中包括As、Cr、Ge、V等18种微量、痕量元素的ICP-MS方法。地化试样用HF-HNO3混酸分解后,以1 1 HNO3溶解干渣。由于制样不使用盐酸,避免了Cl对As、Cr、Ge、V的质谱干扰。用国家一级地球化学标准物质GBW 07309制备溶液优化仪器工作参数,并用于校准。方法测定限(6s)为:0.007~6.4μg/g,精密度(RSD%,n=12)为:29%~9.4%,经过国家一级地球化学标准物质的分析验证,结果与标准值吻合。方法已应用于国土资源调查的试样分析。  相似文献   

14.
15.
以大分子引发剂氯乙酰化聚苯乙烯微球(PS-acyl-Cl)经原子转移自由基聚合(ATRP)法引发丙烯酰胺(AM)和甲基丙烯酸缩水甘油酯(GMA)单体的共聚接枝,制得一种触角状亲水性环氧载体(PS-acyl-g-P(AM-co-GMA)),再经二乙醇胺(DEA)的环氧基开环胺化反应,得到一种含多个-NCH2CH2OH螯合配基的多齿-五元螯合环的触角状亲水性羟胺树脂(PS-acyl-g-P(AM-co-GMA)-DEA)。将此树脂用于硼吸附研究,结果表明,PS-acyl-g-P(AM-co-GMA)-DEA树脂对硼的吸附满足Langmuir方程,为单分子层吸附;饱和吸附量约为37.7 mg·g-1,且树脂5 min即可达到吸附平衡,与其它已报道的吸硼树脂相比,该树脂具有更高的吸附量和吸硼速率。吸附动力学研究表明,树脂吸附硼的过程主要由颗粒扩散过程控制。重复使用5次后该树脂的吸附量基本不变,解吸率均在90%以上,重复使用性能良好。  相似文献   

16.
收集了2001年7月到2002年6月有关国外塑料工业的相关期刊资料,介绍了2001年到2002年国外塑料工业的发展情况,提供了世界各地域塑料原材料的产量及构成比,日本、美国、加拿大、德国、法国、比利时、墨西哥、芬兰、西班牙等国家的树脂产量、消费量及增长率,以及日本、西欧、北美等地区的不同品种塑料原料消费量和增长率统计.按通用热塑性树脂(聚乙烯、聚丙烯、聚苯乙烯、聚氯乙烯、ABS树脂)、工程塑料(尼龙、聚碳酸酯、聚甲醛、热塑性聚酯、聚苯醚)、通用热固性树脂(酚醛、聚氨酯、不饱和树脂、环氧树脂)、特种工程塑料(聚苯硫醚、液晶聚合物、聚醚醚酮)不同品种的顺序,对树脂的产量、消费量及合成工艺、产品应用开发、树脂品种的延伸及应用的进一步扩展等有关技术作了详细的介绍.  相似文献   

17.
工业生产中物位测量的探讨与研究   总被引:4,自引:0,他引:4  
在工业生产中常常会遇到常温,常压和一般介质的液位,料位和界面的测量,也会遇到高温,高压,易燃易爆,腐蚀性较强的液位,料位和界面的测量。在工业生产中物位测量有接触式和非接触式测量。但应根据生产工况及技术要求来合理选用。  相似文献   

18.
19.
The suitability of confocal laser scanning microscopy (CLSM) in examining a wood-coating interface was evaluated using a clear coating system. A comparison of the images of the wood-clear coating interface obtained using CLSM and light microscopy (LM) showed a marked superiority of CLSM in revealing the details of the physical nature of the interaction between the clear coating and the wood cell walls in the surface layer. The most distinct advantage of CLSM was in its ability to clearly resolve penetration of the coating into very fine cracks in cell walls, details not obtainable with LM. The information presented here demonstrates that CLSM has the potential to greatly enhance our understanding of the physical aspects of an interaction between the wood and coating at the interface.  相似文献   

20.
研究了炭黑/白炭黑填充的苯乙烯/乙烯基含量不同的充油溶聚丁苯橡胶(HPR 757 D和Buna VSL 5025-2 HM)的物理机械性能及动态力学性能,观察了填料在硫化胶中的微观分布情况。结果表明,炭黑与白炭黑相互镶嵌地分布在橡胶基质中,形成交织的填料网络。高苯乙烯基含量的HPR 757 D的拉伸强度、撕裂强度及耐磨性能优异,滚动阻力较小,填料与橡胶间的结合力强,填料的分散性较好。用白炭黑等量取代炭黑可以提高胶料的拉伸强度,降低其动态压缩温升。但炭黑/白炭黑的最佳配比与橡胶基质的分子结构有关,主链双键含量越高,白炭黑的用量也随之增多。  相似文献   