以甲基丙烯酸和丙烯酰胺为功能单体,通过悬浮聚合法制备了氨基和羧基双功能化的磁性复合微球(Fe3 O4@SiO2-NH2/COOH),并探讨了其对水溶液中Cd(Ⅱ)和Pb(Ⅱ)的吸附性能.X-射线衍射(XRD)分析表明,制备的磁性吸附剂内核为Fe3 O4.红外光谱(FT-IR)和扫描电镜(SEM)测试表明,氨基和羧基对Fe3 O4@SiO2表面改性成功.吸附试验显示,Fe3O4@SiO2-NH2/COOH吸附Cd(Ⅱ)和Pb(Ⅱ)的最优pH值分别为5.0和5.5,吸附过程均符合动力学准二级模型和Langmuir吸附等温模型,吸附剂对Cd(Ⅱ)和Pb(Ⅱ)最大吸附量分别为207.807 mg/g和168.995 mg/g.实际饮用水样中Cd(Ⅱ)和Pb(Ⅱ)的吸附表明,去除率分别可达97.74%和91.44%.该磁性吸附剂对两种重金属离子吸附量大、去除率高,具有良好的实际应用潜力.  相似文献   

2.
采用改进St?ber法制备超顺磁Fe3O4@SiO2复合粒子作为催化剂载体,再通过浸渍法将H3PW12O40(HPW)负载在Fe3O4@SiO2载体上,制备了一系列超顺磁负载型催化剂HPW/Fe3O4@SiO2。并使用X射线衍射(XRD)、傅里叶红外(FT-IR)、氨的程序升温脱附(NH3-TPD)、扫描电镜(SEM)、N2吸附-脱附和振动样品强磁计(VSM)对催化剂进行表征。结果表明,HPW固定并均匀分散在Fe3O4@SiO2载体上,40%HPW/Fe3O4@SiO2催化剂具有较高的饱和磁强度(30.1 emu·g?1)和较大的比表面积(303.6 m2·g?1),并可用外加磁场进行分离。采用40%HPW/Fe3O4@SiO2催化噻吩与1-辛烯组成的模拟汽油的烷基化脱硫反应,在160℃下反应2 h,噻吩转化率达到85.5%,有较好的催化脱硫性能,且可以多次循环利用。  相似文献   

3.
采用丙烯酸(AA)、丙烯酰胺(AM)、苯乙烯(St)制备了高吸附性的水凝胶[(P(AA-AM-St)],再将SiO2包裹的Fe3O4(Fe3O4@SiO2)与P(AA-AM-St)复合制备了磁性水凝胶[P(AA-AM-St)/Fe3O4@SiO2],研究了其热稳定性、重复利用性,以及吸附条件对其吸附性能的影响,并分析了...  相似文献   

4.
采用氧化法和正硅酸乙酯水解法制备了Mn3O4@SiO2核壳结构磁性纳米材料,研究了其对水溶液中Mo(VI)离子的吸附效果。运用X射线衍射仪(XRD)、扫描电镜(SEM)、透射电镜(TEM)、红外光谱仪(IR)及磁强计(VSM) 等多种手段对Mn3O4@SiO2核壳磁性复合材料进行了表征,并研究了溶液的初始pH、Mo(VI)离子初始浓度和温度对Mo(VI)吸附量的影响。结果表明:在298 K条件下Mn3O4@SiO2核壳结构磁性复合材料对Mo (VI)的饱和吸附量为145.35 mg/g; Mn3O4@SiO2对Mo (VI)的吸附过程符合Langmuir等温吸附模型,吸附动力学符合准二级动力学模型;吸附热力学分析表明Mn3O4@SiO2复合材料对Mo (VI) 的吸附行为是自发的、放热过程。  相似文献   

5.
程昌敬  刘东  张嫦 《化工进展》2012,31(1):227-232
先通过硅酸钠水解在磁性Fe3O4纳米粒子表面包覆二氧化硅,制得磁性硅粒子(Fe3O4@SiO2);然后再通过碳二亚胺活化接枝法在Fe3O4@SiO2纳米粒子表面接枝高脱乙酰度羧甲基化壳聚糖(CMC),制备了一种新型磁性纳米吸附剂(Fe3O4@SiO2@CMC)。通过透射电镜(TEM)、红外光谱(IR)、X射线衍射(XRD)以及振动样品磁强计(VSM)对其进行了表征,着重研究了其对水中Cr(Ⅵ)离子的吸附性能。结果表明:溶液的pH值能显著影响吸附剂对Cr(Ⅵ)离子的吸附效果,pH值为2时效果最佳。结合相应pH值下Cr(Ⅵ)的形态分布,探讨了这种新型材料对Cr(Ⅵ)的吸附机理。结果表明:其吸附机理及吸附容量与Cr(Ⅵ)的离子形式有关,吸附过程以离子交换与静电引力为主。吸附平衡数据分别采用了Langmuir和Freundlich方程进行拟合。结果表明,等温吸附数据更符合Langmuir模型,T=298 K、pH=2、V=5 mL时,吸附剂的饱和吸附容量qm=86.96 mg/g,吸附常数为0.0174 L/mg。  相似文献   

6.
以CS(壳聚糖)和双醛淀粉为反应原料,制备了吸附苯酚用CS双醛淀粉希夫碱。着重探讨了合成希夫碱的影响因素、希夫碱对苯酚的吸附动力学过程。研究结果表明:当n(CS)∶n(双醛淀粉)=2∶3、反应温度为70℃和反应时间为12 h时,制得的希夫碱具有相对最大的接枝率(65.4%);希夫碱对苯酚的吸附速率随吸附时间延长而逐渐下降,80 min时达到饱和吸附;当吸附质浓度为20 mg/L、吸附剂浓度为500 mg/L和吸附剂为0.05 g时,饱和吸附量为32.015 mg/g;拟1级、拟2级吸附动力学方程均具有良好的线性相关性,并且前者的拟合效果相对更好。  相似文献   

7.
采用壳聚糖材料为吸附剂,通过水热氧化-溶胶凝胶方法制备了纳米级Fe3O4@SiO2@CTS颗粒(MCNPs)。这种新型吸附剂对Cd2+和Cu2+的吸附在2 min内就可完成,其饱和吸附容量分别为110.0、89.1 mg/g,且能够通过酸洗脱附,脱附率分别达到92.7%和94.6%;3次回用后吸附容量仍能达到92.2、79.8 mg/g;经60℃水浴处理0.5 h后吸附率仅分别下降1.9%和1.4%;而且该吸附剂具有较大的饱和磁化强度(13.3 Am2/kg)和很小的矫顽力(1.4 mT),可通过磁性快速回收,并在水中分散性良好。可见,MCNP是一种可回收再利用、可满足重金属应急污染处理要求的吸附剂。  相似文献   

8.
《腐植酸》2015,(4)
本研究合成了腐植酸(HA)包裹的Fe3O4纳米颗粒(Fe3O4/HA)并将其用于去除水中的重金属离子,包括Hg(I)、Pb(I)、Cd(I)和Cu(I)。以价格低廉、环境友好的铁盐和腐植酸为原料,通过共沉淀方法制备Fe3O4/HA。TOC和XPS的分析结果表明所制备的Fe3O4/HA中约含有11%(w/w)的叶酸,它是含O和N-官能团丰富的组分。TEM成像和激光颗粒尺寸分析证实所制备的Fe3O4/HA(Fe3O4内核约为10 nm)在水溶液中团聚并形成了平均水和半径约为140 nm的聚集体,饱和磁化强度为79.6 emu/g,这种Fe3O4/HA材料在低磁场梯度下几分钟内就可以从水溶液中分离。Fe3O4/HA对重金属离子的吸附在15分钟内就可以达到平衡,其吸附行为符合朗格缪尔吸附模型,且最大吸附容量在46.3~97.7 mg/g范围内。制备的Fe3O4/HA在自来水、天然水、0.1 M HCl和2 M Na OH的酸/碱溶液中都很稳定,Fe(≤3.7%)和HA(≤5.3%)的泄漏率很低。在最优条件下,Fe3O4/HA纳米材料能够去除天然水和自来水中超过99%的Hg(II)和Pb(II)以及超过95%的Cu(II)和Cd(II)。Fe3O4/HA吸附的重金属离子泄露回水溶液的量几乎可以忽略。  相似文献   

9.
用共沉淀法制备出具有磁性的Fe3O4纳米粒子水溶液。红外光谱和XRD表明,纳米粒子是Fe3O4且其粒径在15 nm左右。通过磁滞回线得到纳米粒子比饱和磁化强度σr=56.58 emu/g。对PET薄膜进行预处理和阴离子化后,在PET表面交替吸附聚电解质聚二甲基二烯丙基氯化铵(PDDA)和纳米粒子水溶液,由于PDDA的存在,Fe3O4纳米粒子能均匀地被吸附在PET表面,形成PET基磁性膜材料,且吸附的强度较强。该材料的矫顽力为41.11 Oe,剩余磁化强度为0.66 emu,与Fe3O4纳米粒子一样,具有超顺磁性。  相似文献   

10.
采用不同方法对粉煤灰进行改性,并将改性粉煤灰用于模拟含磷废水的处理。实验结果表明:酸(H_2SO_4、HNO_3、HCl)、碱(Na OH)和盐(Fe Cl_3)改性粉煤灰对磷的吸附效果相较于原粉煤灰都有一定程度上的增强。其中,Fe Cl_3改性粉煤灰对磷的吸附效果最好,吸附达到平衡时,最大吸附量达到328μg/g,且当循环吸附6次后吸附量仍可达到303μg/g。Fe Cl_3改性粉煤灰对磷的吸附符合Langmuir吸附等温线模型,吸附过程是吸热的。  相似文献   

11.
It is well established that a wide range of drugs of abuse acutely boost the signaling of the sympathetic nervous system and the hypothalamic–pituitary–adrenal (HPA) axis, where norepinephrine and epinephrine are major output molecules. This stimulatory effect is accompanied by such symptoms as elevated heart rate and blood pressure, more rapid breathing, increased body temperature and sweating, and pupillary dilation, as well as the intoxicating or euphoric subjective properties of the drug. While many drugs of abuse are thought to achieve their intoxicating effects by modulating the monoaminergic neurotransmitter systems (i.e., serotonin, norepinephrine, dopamine) by binding to these receptors or otherwise affecting their synaptic signaling, this paper puts forth the hypothesis that many of these drugs are actually acutely converted to catecholamines (dopamine, norepinephrine, epinephrine) in vivo, in addition to transformation to their known metabolites. In this manner, a range of stimulants, opioids, and psychedelics (as well as alcohol) may partially achieve their intoxicating properties, as well as side effects, due to this putative transformation to catecholamines. If this hypothesis is correct, it would alter our understanding of the basic biosynthetic pathways for generating these important signaling molecules, while also modifying our view of the neural substrates underlying substance abuse and dependence, including psychological stress-induced relapse. Importantly, there is a direct way to test the overarching hypothesis: administer (either centrally or peripherally) stable isotope versions of these drugs to model organisms such as rodents (or even to humans) and then use liquid chromatography-mass spectrometry to determine if the labeled drug is converted to labeled catecholamines in brain, blood plasma, or urine samples.  相似文献   

12.
13.
建立了测定地球化学样品中包括As、Cr、Ge、V等18种微量、痕量元素的ICP-MS方法。地化试样用HF-HNO3混酸分解后,以1 1 HNO3溶解干渣。由于制样不使用盐酸,避免了Cl对As、Cr、Ge、V的质谱干扰。用国家一级地球化学标准物质GBW 07309制备溶液优化仪器工作参数,并用于校准。方法测定限(6s)为:0.007~6.4μg/g,精密度(RSD%,n=12)为:29%~9.4%,经过国家一级地球化学标准物质的分析验证,结果与标准值吻合。方法已应用于国土资源调查的试样分析。  相似文献   

14.
15.
以大分子引发剂氯乙酰化聚苯乙烯微球(PS-acyl-Cl)经原子转移自由基聚合(ATRP)法引发丙烯酰胺(AM)和甲基丙烯酸缩水甘油酯(GMA)单体的共聚接枝,制得一种触角状亲水性环氧载体(PS-acyl-g-P(AM-co-GMA)),再经二乙醇胺(DEA)的环氧基开环胺化反应,得到一种含多个-NCH2CH2OH螯合配基的多齿-五元螯合环的触角状亲水性羟胺树脂(PS-acyl-g-P(AM-co-GMA)-DEA)。将此树脂用于硼吸附研究,结果表明,PS-acyl-g-P(AM-co-GMA)-DEA树脂对硼的吸附满足Langmuir方程,为单分子层吸附;饱和吸附量约为37.7 mg·g-1,且树脂5 min即可达到吸附平衡,与其它已报道的吸硼树脂相比,该树脂具有更高的吸附量和吸硼速率。吸附动力学研究表明,树脂吸附硼的过程主要由颗粒扩散过程控制。重复使用5次后该树脂的吸附量基本不变,解吸率均在90%以上,重复使用性能良好。  相似文献   

16.
收集了2001年7月到2002年6月有关国外塑料工业的相关期刊资料,介绍了2001年到2002年国外塑料工业的发展情况,提供了世界各地域塑料原材料的产量及构成比,日本、美国、加拿大、德国、法国、比利时、墨西哥、芬兰、西班牙等国家的树脂产量、消费量及增长率,以及日本、西欧、北美等地区的不同品种塑料原料消费量和增长率统计.按通用热塑性树脂(聚乙烯、聚丙烯、聚苯乙烯、聚氯乙烯、ABS树脂)、工程塑料(尼龙、聚碳酸酯、聚甲醛、热塑性聚酯、聚苯醚)、通用热固性树脂(酚醛、聚氨酯、不饱和树脂、环氧树脂)、特种工程塑料(聚苯硫醚、液晶聚合物、聚醚醚酮)不同品种的顺序,对树脂的产量、消费量及合成工艺、产品应用开发、树脂品种的延伸及应用的进一步扩展等有关技术作了详细的介绍.  相似文献   

17.
工业生产中物位测量的探讨与研究   总被引:4,自引:0,他引:4  
在工业生产中常常会遇到常温,常压和一般介质的液位,料位和界面的测量,也会遇到高温,高压,易燃易爆,腐蚀性较强的液位,料位和界面的测量。在工业生产中物位测量有接触式和非接触式测量。但应根据生产工况及技术要求来合理选用。  相似文献   

18.
19.
The suitability of confocal laser scanning microscopy (CLSM) in examining a wood-coating interface was evaluated using a clear coating system. A comparison of the images of the wood-clear coating interface obtained using CLSM and light microscopy (LM) showed a marked superiority of CLSM in revealing the details of the physical nature of the interaction between the clear coating and the wood cell walls in the surface layer. The most distinct advantage of CLSM was in its ability to clearly resolve penetration of the coating into very fine cracks in cell walls, details not obtainable with LM. The information presented here demonstrates that CLSM has the potential to greatly enhance our understanding of the physical aspects of an interaction between the wood and coating at the interface.  相似文献   

20.
研究了炭黑/白炭黑填充的苯乙烯/乙烯基含量不同的充油溶聚丁苯橡胶(HPR 757 D和Buna VSL 5025-2 HM)的物理机械性能及动态力学性能,观察了填料在硫化胶中的微观分布情况。结果表明,炭黑与白炭黑相互镶嵌地分布在橡胶基质中,形成交织的填料网络。高苯乙烯基含量的HPR 757 D的拉伸强度、撕裂强度及耐磨性能优异,滚动阻力较小,填料与橡胶间的结合力强,填料的分散性较好。用白炭黑等量取代炭黑可以提高胶料的拉伸强度,降低其动态压缩温升。但炭黑/白炭黑的最佳配比与橡胶基质的分子结构有关,主链双键含量越高,白炭黑的用量也随之增多。  相似文献   